Question posted - February 12 to February 16, 2018:

Can efflorescence be removed from integrally colored CMU without damaging the appearance? How?



More items for Maintenance + Renovation


Selected Answers

From Brian Trimble of IMI on February 14, 2018:
I would agree with Zenith Czora's recommendations except when cleaning "insoluble efflorescence" (which I would call lime run or calcium carbonate deposits). I have seen too many walls damaged with inappropriate high-pressure cleaning. It can be done right, but there are specific proprietary cleaners for calcium carbonate stains that should be considered first.

From Zenith Czora of Zen Consultancy on February 12, 2018:
First of all, the efflorescence that is existing on the CMU surface needs to be assessed. Efflorescence does cause discoloration of the affected surface. Determine whether it is a primary efflorescence (whitish bloom or color fade), which develops during setting and curing of the CMU, or a secondary efflorescence ( uniform discoloration or localized encrustations), which develops later where moisture or water exits the CMUs. Or  it may be a cryptoflorescence, which is a salt crystallized within the pore structures of the CMUs. It forms below the surface and is not visible until the crystal growth develops enough to cause surface scaling and spalling. There are two methods of removing efflorescence. Chemical removal uses diluted acid like acetic acid, citric acid or phosphoric acid, but it may alter the surface color and texture. (Bear in mind that efflorescence also causes discoloration.) and then the treated surface may be neutralized with 10% ammoniacal solution or KOH.  Mechanical removal by dry brushing can remove fresh deposits of water-soluble efflorescence using a stiff bristle brush and vacuuming the loosened materials from the substrates and surrounding surfaces..Wet brushing can be used if dry brushing is ineffective, provided there is no opportunity for salt redepositing back on the surface when water evaporates. High-pressure water jetting can be used for insoluble efflorescence. If the sources of efflorescence--soluble salts, water/moisture in contact with the salts forming salt solutions, and a passage allowing salt solution to migrate to the surface--are not minimized or at least one is eliminated, efflorescence may possibly reoccur.


Please sign in to submit your answer this question

   

Tagged categories: Efflorescence


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Shield Industries, Inc
 
FireGuard® E-84 Intumescent Coating - Shield Industries, Inc
 
Trust the certified protection of the industry’s most innovative intumescent coating FireGuard® E-84 to provide you with the 1 and 2 hour fire ratings you need.
 

 
Novatek Corporation
 
Novatek Portable Air Filtration Systems
 
Air Scrubbers/Negative Air machines for restoration, abatement, dust & odor control, hazardous contaminant removal from job sites to clean rooms and hospitals. Portable, affordable!
 

 
Keim Mineral Coatings
 
Mineral Silicate Paints + Stains Fuse to Concrete
 
• Forms permanent chemical bonds
• Becomes part of the concrete
• Will never peel
• Looks completely natural
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@durabilityanddesign.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 

© Copyright 2012-2018, Technology Publishing Co., All rights reserved